> Hot Rolled

DD11

BS EN 1011:2008 DD11. Dry or pickled and oiled.

 

Yield Strength:    1.5mm – 1.99mm 170 – 360 Mpa
  2.0mm – 7.00mm 170 – 340 Mpa
  270 – 500 Mpa
Tensile strength       

 

Max. chemical composition % by mass
Carbon 0.12
Manganese 0.60
Phosphorus 0.10
Sulphur 0.045

 

> View properties for S275