S275 complying with BS EN 10025 – 2: 2004 S275
Formerly known as 4360/43a.

 

Yield Strength:    <16mm: 275 Mpa
Tensile strength:      <3mm: 430 – 580 Mpa
  >3mm: 410 – 560 Mpa
      

 

Max. chemical composition % by mass
Carbon 0.25
Silicon 0.5
Manganese 1.60
Phosphorus 0.0050
Sulphur 0.050

 

 